SMSI is typically triggered by high-temperature treatments in a reductive atmosphere (such as H2). The reduction of the support material (often a metal oxide) results in migration of the reduced species over the metal particles. This phenomenon is particularly prominent in reducible oxides such as TiO2, which undergoes a structural transformation at elevated temperatures, facilitating the interaction with the metal catalyst.