What can Differential Scanning Calorimetry (DSC) tell us about Catalysts?
Differential Scanning Calorimetry (DSC) measures the heat flow associated with chemical reactions and phase transitions in catalysts. It helps in understanding the thermal stability and the energetic aspects of catalytic processes.