Co-Mo catalysts are typically prepared by impregnation methods, where cobalt and molybdenum precursors are deposited onto a high-surface-area support material, such as alumina. The impregnated material is then dried, calcined, and sometimes reduced to activate the catalyst. The precise preparation conditions can significantly influence the final catalytic properties.